单模块 MFSC-2000X-50um 切割数据

Single module MFSC-2000X-50um cutting data

三、单模块 MFSC-2000X 切割数据  Single module MFSC-2000X-50um cutting data

3.1 创鑫单模块 MFSC-2000X QBH 输出纤芯 50 μm 切割数据(准直 100mm/聚焦 125mm)Single module MFSC-2000X QBH output fiber core 50μm cutting data (collimation 100mm/ focus 125mm)


MFSC-2000X 连续激光器(50μm)

MFSC-2000X Continuous Laser (50μm)

材料Material

厚度 thicknes

(mm)

速度Speed

(m/min)

功率

Power

(W)

气体

Gas

气压

Pressure

(bar)

喷嘴Nozzles

(mm)

焦点位置

Focus

Point

(mm)

喷高Height

of

blowout

(mm)

碳钢Carbon

Steel

1

25-30

2000

N2/

Air

10

2.0 单Single

0

0.6

2

6-8

10

2.0 单Single

-1

0.5

2

5-6

2000

O2

1.5

1.0 双Single

+3

0.6

3

3-4

0.8

1.0 双Single

+4

0.6

4

2.5-3.0

0.8

1.0 双Single

+4

0.6

5

2.2-2.6

0.6

1.0 双Double

+5

0.6

6

1.8-2.0

0.6

1.0 双Double

+6

0.8

8

1.2-1.6

0.6

1.2 双Double

+5.5

0.8

10

1.0-1.2

0.6

1.2 双Double

+5

0.8

12

0.8-1.0

0.6

4.0 双Double

+4

1.0

14

0.7-0.85

0.6

4.0 双Double

+4

1.0

16

0.6-0.7

0.6

4.0 双Double

+4

1.0

18

0.5-0.6

0.6

5.0 双Double

+4

1.0

20

0.4-0.5

0.6

5.0 双Double

+4

1.0

不锈钢

1

28-35



10

2.0 单Single

0

0.5

Stainles

s Steel

2

9.0-15

2000

N2

10

2.0 单Single

-1

0.5

3

6.0-7.0

12

3.0 单Single

-1.5

0.5

4

2.8-3.5

14

3.0 单Single

-2

0.5

5

1.5-2.5

15

3.0 单Single

-3

0.5

6

1.0-1.5

16

3.5 单Single

-4

0.5

8

0.7-0.9

18

4.0 单Single

-5

0.5

铝合金Alumini

um

Alloy

1

22-35

2000

N2

12

2.0 单Single

0

0.5

2

8.0-13

12

2.0 单Single

-0.5

0.5

3

4.0-4.5

14

3.0 单Single

-1

0.5

4

2.5-3.0

15

3.0 单Single

-2

0.5

5

1.5-2.0

16

3.0 单Single

-3

0.5

6

0.8-1.3

16

3.5 单Single

-4

0.5

黄铜

Brass

1

15-18

2000

N2

10

2.0 单Single

0

0.8

2

6.0-8.0

10

2.0 单Single

-1

0.5

3

2.5-3.0

12

3.0 单Single

-1.5

0.5

4

1.0-1.3

13

3.0 单Single

-2

0.5

5

0.7-0.8

14

3.5 单Single

-2.5

0.5

紫铜Copper

1

20-22

2000

O2

12

3.0 单Single

-1

0.5


2

5.5-6.5



12

3.0 单

-1

0.5

3

2.0-3.0

14

3.0 单Single

-2

0.5

备注:碳钢和不锈钢等空气、氮气切割时,效率和稳定性都会提升,承着厚度增加,也容易出现挂渣现象,上面数据参数在实际批量切割时,受机床、系统、切割头、气压、材料等因素影响,数据可能会有变动,表中红标参数为打样参数,在实际加工中受各类因素影响较大,仅适合小批量生产,不推荐大批量生产加工,建议使用更高功率激光器。紫铜需用高压氧气切割,空气或氮气易造成激光器损坏。

Remark: Carbon steel and stainless steel, such as air, nitrogen cutting, efficiency and stability will be improved, bearing the increase of thickness,  but also  prone to hanging slag  phenomenon, the above data parameters in actual bulk cutting, machine tool, system, cutting head, air pressure, materials and other factors, there may be changes, the data in the table red mark parameters for proofing, greatly influenced by various factors in the actual processing, It is only suitable for small batch production.  Mass production is not recommended.  Higher power lasers are recommended. Copper needs to be cut with high pressure oxygen, air or nitrogen are easy to cause damage to the laser.

3.2 单模块 MFSC-2000X 纤 芯 50 μ m 穿孔推荐 Single  module  MFSC-2000X fiber core 50μm perforation reference

3.2.1 创鑫 MFSC-2000X 20mm 碳钢氧气穿孔参数(仅供参考) MAX  MFSC-2000X 20mm carbon steel oxygen perforation parameters (for reference only)

阶段Stage

功率

Power

(W)

占空比duty

ratio

(%)

频率Frequ

ency

(Hz)

喷嘴高度Nozzles

Height

(mm)

气压

Air

Pressu

re

(bar)

焦点

Focus

Point

(mm)

穿孔时间Aperture

Time

(ms)

停光吹气

Stop

blowing

(ms)

高位High-po

sition

2000

55

100

20

0.8

-2

200


中位Middle-

position

2000

45

100

15

0.7

-4

1000


低位 Low-pos

ition

2000

55

100

8

0.6

-6

2000


3.2.2 创鑫 MFSC-2000X 8mm 不锈钢氮气穿孔参数(仅供参考) Nitrogen perforation parameters of MAX MFSC-2000X 8mm stainless steel (for reference only)


阶段stage

功率

Power

(W)

占空比duty

ratio

(%)

频率Frequ

ency

(Hz)

喷嘴高度Nozzles

Height

(mm)

气压

Air

Pressu

re

(bar)

焦点

Focus

Point

(mm)

穿孔时间Aperture

Time

(ms)

停光吹气

Stop

blowing

(ms)

高位High-po

sition

2000

55

2500

16

10

-2

200


中位Middle-

position

2000

50

2500

12

10

-4

1000


低位 Low-pos

ition

2000

40

2000

8

10

-6

500


穿孔参数以当前功率下能够穿透的极限碳钢/不锈钢厚度为例,穿孔参数可调节范围大,依据实际效果可调节占空比和频率等参数,达到最佳效果;穿孔按顺序逐级排序,高位为第一级穿孔,以此类推。

The  perforation  parameters  are  taken  as  the  limit  carbon  steel/stainless  steel  thickness  that  can  be penetrated under the current power as an example. The perforation parameters can be adjusted in a wide range, and the duty cycle and frequency can be adjusted according to the actual effect to achieve the best effect. The piercings are sorted step by step, the high position is perforated for the first level, and so on.


咨询 HEAVTH 数控专家
用我们的专业为您提供数控切割和焊接所需的产品和服务。
我们提供产品尺寸、电气性能、外观设计、操作界面等方面来定制设备。

我们可以提供什么

我们做什么

我们的技术

服务

© 版权所有 2024 常州海斯科技有限公司版权所有。